Features:
●Hard anodizing for piston.
Parameter:
Item |
Unit |
|
|
Capacity |
Piston
diameter range |
mm |
60-100 |
Piston
height range |
mm |
40-80 |
|
Productivity- Ring groove oxidation |
– |
≤120s |
|
Productivity- Crown oxidation |
– |
≤360s |
|
Features |
Ⅰland +1 Groove area + Partial top land |
– |
Standard
configuration |
Ⅰland +1 Groove area + entire top land |
– |
Standard
configuration |
|
Ⅰland +1 Groove area + entire top land
+Out diameter of top land |
– |
Standard
configuration |
|
Washing
machine |
– |
Optional |
|
Equipment accuracy |
Ring
groove oxide layer thickness |
μm |
15±5 |
Roughness |
μm |
Ra≤2 |
|
Oxide
layer hardness (Vickers hardness) |
– |
HV350±50 |
|
Other |
Power
supply |
V/Hz |
440/50 |
Air
pressure |
Bar |
2-10 |
|
Total
power |
Kw |
100 |
|
Net
weight |
Kg |
3000 |